Einleitung

    • Go to kisslicer

    • go to style

    • Adjust the infill density

    • Adjust Infill extrusion width and Infill style

    • Open kisslicer

    • Increase the skin thickness

    • skin thickness=Extrusion width *no of loops

    • Go to control in machine menu

    • Click Temperature

    • Go to nozzle 1 and and increase the temperature by 5 degree

    • Go to main menu

    • If you Rotate the knob in anti clock wise direction, the speed will be decreasing.

    • Decrease the speed by 20%

Abschluss

To reassemble your device, follow these instructions in reverse order.